| View single post by runfiverun | |||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Posted: Sun Jun 28th, 2009 07:18 PM |
|
||||||||||||
runfiverun
|
i grab as much as i can and try to go over to the range about once a month just to pick up lead. i usually get about a 5 gal bucket in a years time. i like to sort mine back out as i go, along with the cast stuff. i thro the plated jacketed and obvious b/p stuff together and put it in a separate bucket. i mix this up with ww's at about 25% range to 75% ww's it is great for the levers and handguns,it's also awesome for lowering the antimonial wash in rifle bbls after being water dropped.
|
||||||||||||
| |||||||||||||